Revision 11/02/2017      

FORMULA 9-L
Language: English



Thermbond Refractories use the patented Stellar Binder Systemâ„¢ for easy and accurate mixing, controlled setting, fast dry-out and heat up, thermal shock resistance and other unique properties. Thermbond chemically bonds to existing fired refractories.

CHARACTERISTICS - Silica - Mullite - Fast Curing - Longer Working Time - Fast Setting - Dense


 

PACKAGING

Unit Equivalent Bags:1 Jug:1
Bag Weight* 60 lbs 27.2 kg
Jug Weight* 8 lbs 3.6 kg
Drum Weight 400 lbs 181.4 kg
Unit Weight* 68 lbs 30.9 kg
Yield / Unit* 0.45 ft3 0.013 m3
Units / Ton* 29.34 short 32.34 metric
Wet to Dry Ratio* Contact us for details
Liquid Activator FORMULA
Bags Per Pallet 48
Drums Per Dry Pallet 1
 

COMPRESSIVE STRENGTH**

1500F (816C) 3000 psi 211 kg/cm2 20.7 N/mm2
2000F (1093C) 5000 psi 352 kg/cm2 34.5 N/mm2
2500F (1371C) 5500 psi 387 kg/cm2 37.9 N/mm2
 

CHEMICAL ANALYSIS (After 1500F (816C))**

  • Al2O3
  • SiO2
  • Fe2O3
  • P2O5
  • Other
  • Total
  • 57.00 %
  • 34.00 %
  • 0.80 %
  • 5.00 %
  • 3.20 %
  • 100.00 %
 

COLD MODULUS OF RUPTURE**

1500F (816C) 800 psi 56 kg/cm2 5.5 N/mm2
2000F (1093C) 1100 psi 77 kg/cm2 8 N/mm2
2500F (1371C) 1200 psi 84 kg/cm2 8 N/mm2
 

HOT MODULUS OF RUPTURE**

1500F (816C) 1800 psi 127 kg/cm2 12 N/mm2
 

APPLICATION

Data based on
  • Casting
 

BULK DENSITY**

As Placed 150 lbs/ft3 2403 kg/m3
After 1500F (816C) 140 lbs/ft3 2243 kg/m3
 

PERMANENT LINEAR CHANGE**

1500F (816C) -0.35%
2000F (1093C) -0.40%
2500F (1371C) 0.30%
 

THERMAL CONDUCTIVITY**

600F (316C) 8.5 Btu-in/hr-ft2-F 1.23 W/m K
1000F (538C) 8.7 Btu-in/hr-ft2-F 1.25 W/m K
1200F (649C) 9.1 Btu-in/hr-ft2-F 1.31 W/m K
1800F (982C) 9.5 Btu-in/hr-ft2-F 1.37 W/m K
**Test data shown are based on averages subject to normal variation on individual tests, and therefore should not be assumed to be maximum or minimum specifications.
***Application by alternative method may produce somewhat different results.
Measures are approximate and may vary. For mixing partial units, contact Stellar Materials for specific wet-to-dry ratios. See Installation Guide for more detailed information.
To assure you are getting the latest data, see our online data sheets at tds.thermbond.com.
Due to the unique nature of the Stellar binder system, test procedures vary slightly from ASTM.
Documentation of these variations is available upon request.
Thermbond is a registered trademark of Stellar Materials Incorporated. All rights reserved.